The use of cored wires for thermal spraying is a relatively new development that is being rapidly utilized for arc spray in a wide variety of applications. This paper will discuss the existing applications and industries in which cored wire coatings are used. Additionally, this presentation will cover the effect cored wires have had on the use of other types of thermal spray equipment. The paper will close with a trend analysis that discusses the applications of the future.