Abstract
Plasma transferred arc (PTA) welding is widely used in the petroleum and chemical industry to deposit nickel and cobalt-based materials on key parts for the purpose of surface modification. As test results show, the process improves corrosion, wear, and high-temperature resistance, prolonging the service life of components and equipment and reducing production costs.
This content is only available as a PDF.
Copyright © 1998 ASM International. All rights reserved.
1998
ASM International
Issue Section:
Industrial Applications
You do not currently have access to this content.