Abstract
This article discusses the influence of refrigerants on the cooling of thermal spray equipment. The discussion covers the cooling requirement for thermal spray equipment, basic cooling systems, improvement and adaptation of refrigerants, challenges for manufacturers and users of cooling technology, and ways to address the challenges.