Abstract
Thermochemical processes are an appropriate way to improve the surface hardening of the material against wear. Thermal spraying is a group of deposition processes that can deposit different classes of materials. The use of thermomechanical process after metallic coatings deposition can result in a unique combination of bulk and surface properties. There are some studies that indicate the defects and stresses caused in the crystal lattice as one of the factors that most influence nitrogen diffusion during the nitriding process. The HVAF (High Velocity Air-Fuel) process can generate different fault conditions and stress-strain in the crystal lattice. The aim of this work is study the effect of the plasma nitriding or, as it is known, Glow Discharge (GD), on FeMnCrSiNi coating deposited with HVAF process. Initially, it was observed the formation of expanded austenite and CrN on the HVAF coating, followed by important increase on the hardness of the coating.