The agglomeration process plays an important role in suspension plasma spraying (SPS), affecting the state of particles prior to impact and consequently the mechanical properties of the coated substrate. This paper presents the results of an investigation on the agglomeration of submicron YSZ particles sprayed from a water suspension. The shape and surface morphology of transient and final agglomerate structures was studied by injecting YSZ suspensions with a nebulizer into an inductively coupled plasma torch. It was found that particle agglomeration occurs in successive stages identified as cup or doughnut shaped agglomerates, polycrystalline particles, and amorphous or partially molten particles.