Tin coatings have been successfully applied to polymeric substrates by means of cold spraying. In this work, three low melting point powders, including Sn, Sn-Zn, and Sn-Bi, are cold sprayed onto various polymeric substrates and different combinations of gas temperature and pressure are assessed. Based on the results, the effect of melting points on the cold sprayability of feedstock powders is discussed.