This study investigates the feasibility of producing GaN coatings on stainless steel, aluminum, and indium tin oxide glass substrates by downstream injection low-pressure cold spraying. The formation of GaN layers on all three materials appears to be due to pseudo deformation of super agglomerated GaN particles. The deposition results showed a saturation limit to coating thickness with the number of passes. Based on XRD spectra of the coating and powder, no phase transformations took place during the spraying process.