This study investigates the synergistic effects of cavitation and corrosion on Cr3C2-25NiCr coatings with different levels of porosity. The coatings are deposited by HVOF spraying and evaluated based on SEM analysis, Vickers microhardness, potentiodynamic polarization measurements, and cavitation erosion tests in various environments under ultrasonic vibration. The results show that higher porosity reduces both cavitation and corrosion resistance, as expected. However, the samples did not show significant alteration of their cavitation properties in NaCl, probably because of the high corrosion resistance of the different phases in the coating. The influence of HVOF fuel-oxygen ratio and total gas flow on coating porosity, as well as phase morphology, is also discussed.