Metallic implants for orthopedic or dental use are often coated with a plasma-sprayed hydroxyapatite (HA) layer. In this study, HA coatings are applied to titanium substrates of varying thickness and laser shock adhesion tests are performed using different laser spot diameters. The objective is to investigate the effect of different shockwave regimes on interfacial debonding and the potential consequences of laser shock adhesion testing. HA coatings exhibiting different levels of adhesion were subjected to laser shock experiments and subsequently examined using nondestructive inspection techniques. The results are presented along with suggestions for developing a robust laser shock adhesion test.