Abstract
Additive manufacturing (AM) techniques give access to completely new manufacturing processes. AM techniques using metals, ceramics, or plastics feedstock are predestined for lightweight construction and for components with complex shapes or internal functions. AM processing with plastics stands out due to the low density of polymers, a good process capability, and low initial costs. The properties of polymer components are extremely dependent on the utilized plastics and the reinforcements, e.g. in the form of fibres. Furthermore, coatings can improve the properties and enhance the possible range of applications for plastics. In the present study, PLA (polylactic acid) was printed utilizing Fused Layer Modeling (FLM). The surfaces of the PLA samples were directly structured with pits with different widths during printing. Subsequently, the surfaces were coated with ZnAl2 by means of Twin Wire Arc Spraying (TWAS). Adhesion tests meeting DIN EN 582 were conducted to measure the adhesion of the coating on the structured plastic surface. The results were compared to the adhesion of ZnAl2 coatings on grit blasted and as-built surfaces. Overall, the surface adhesion was significantly better for the samples with directly structured surfaces. Hence, a direct structuring of the surface during a 3D building process promises to be an outstanding possibility to prepare surfaces prior to coating processes.