This study investigates the sliding wear behavior of HVOF sprayed coatings derived from conventional, fine, and nanostructured WC-Co powders. The results show that WC-Co coatings produced from fine and nanostructured feedstocks have significantly higher wear resistance and lower friction coefficients than coatings derived from conventional sized powder. This is attributed to scaling effects in the microstructure and phase evolution of the coating material as explained in the paper.