This paper reviews the capabilities of portable low pressure cold spraying systems and presents examples of the repairs that have been made and the different materials involved. It discusses the recent development of ceramic nozzle inserts that extend continuous operating time to more than 10 h and non-pressurized rotating-vibratory powder feeders that provide higher, more stable powder feed rates for production environments.