Abstract
In this study, a nickel-coated Al2O3 powder, produced by hydrothermal hydrogen reduction, is cold sprayed with the aim of increasing the volume fraction of alumina particles in the nickel matrix. Spray trials were conducted to investigate the effect of oxidation temperature on the microstructure and hardness of as-sprayed as well as heat treated Ni-Al2O3 composite coatings. Results show that oxidizing has a significant effect on microstructure and hardness and that the morphologies of oxide films differ depending on the heat treatment.