Abstract
In this study, plain carbon steel wire and pure iron powder are deposited on grit-blasted Fe-Si alloy substrates using thermal (electric arc, plasma, and HVOF) and kinetic spraying techniques. The coatings obtained were then heat treated. Coating microstructures and mechanical properties were investigated and compared focusing on oxidation, delamination, and Si dilution from the substrate to the coating.