Abstract
WC-Co cermet powders were deposited on aluminum substrates by cold gas spraying. XRD tests were run on the powder and coatings to reveal possible phase changes during spraying. Bonding strength, abrasive wear resistance, and corrosion resistance were also measured and are compared with values obtained from HVOF sprayed WC-Co coatings.