Cold Gas Spray allows to extend the range of steel coating formulations in comparison with other thermal spraying techniques because the material doesn’t melt during process. The absence of processes of fast solidification implies the absence of tensile stresses in the coating and makes possible to obtain thick coatings becoming a new alternative to welding cladding processes for the restoration of surfaces with corrosion pitting, notched areas or welded zones with bad appearance and for the repair of porous casting, contractions or losses of tolerance, by applying located coatings. 17-4 PH steel is one of the most widely used precipitation hardening grades in the business, offering high strength with corrosion resistance similar to S30400 in most environments. While soft and ductile in the solution annealed condition, it is capable of high properties with a single precipitation or aging treatment. Characterized by good corrosion resistance, high hardness, toughness and strength. Commonly used in both aircraft and gas turbines, nuclear reactor, paper mill, oil field, and chemical process components. A study has carried out in Thermal Spray Center for the production and optimization of thick coatings of 17-4 PH steel (S17400) through Cold Gas Spray technology onto carbon steel substrates. The study concentrates in the determination of influence of spray parameters on coating properties.

This content is only available as a PDF.
You do not currently have access to this content.