Abstract
Characterization of coatings made with the help of Computer Controlled Detonation Spraying (CCDS) was performed. The applied coatings include hard alloys (WC/Co -75/25, WC/Co - 88/12, WC/Co/Cr - 86/10/4, and Cr2C3 / NiCr), aluminum oxide, nickel-chromium self-fluxing alloy, titanium, bronze, and stainless steel. Tribological investigations of coatings were provided using abrasion test (ASTM standard G65), erosion test (ASTM standard G76), and hydro-abrasive test. To make hydro-abrasive tests special device and method were elaborated based on the interaction of water jet saturated with corundum particles with a coating surface.
This content is only available as a PDF.
Copyright © 2011 DVS Media GmbH. All rights reserved.