Abstract
In order to explore wear properties of Ni-based coating on the copper substrate, the coatings with different composition were designed. Ni-based coating, Ni-based/Al2O3 and Ni-based/Al2O3/WC coatings were sprayed by HVAF on the copper substrates. Wear properties of different composite coating were measured at different loads at room temperature. The experimental results indicate that all the coatings have high wear resistance. Adding Al2O3 in sprayed powders has little effect on the microstructures and wear properties of coating. The wear resistant is improved by the addition WC-12Co obviously. The best wear resistant is obtained when optimum WC-12Co content is added.