Abstract
As the requirements placed on thermal coatings become increasingly stringent, being able to acquire more accurate data more quickly is becoming increasingly important. To achieve this, process variables must be measured close to or even inside the gun. This paper introduces a new product which measures process variables directly inside a thermal spray gun. It explains the advantages of measuring the process variables inside the gun, but also why it is important to have gun-relevant data stored on the gun itself.
Copyright © 2010 DVS Media GmbH. All rights reserved.
2010
DVS Media GmbH
Issue Section:
Process Diagnostics
You do not currently have access to this content.