Abstract
Since the first installation of a cold spray system at OBZ Innovation GMBH in 2002 the application areas of cold spraying have increased greatly. Cold spraying has developed into a safe and reliable process that is used successfully in various areas of industry. In this presentation current applications and new project developments at OBZ Innovation GMBH are demonstrated. Furthermore within an outlook the new possibilities with the latest cold spray technology, the KINETICS-8000-HP, are demonstrated. With this unit it is possible to increase the deposition rate compared to previous cold spray systems and expand the material spectrum usable for cold spraying to include higher refraction materials – all while cutting costs, increasing quality and maintaining excellent process reliability.