Abstract
This paper describes an inner diameter HVOF spraying technique and associated tests methods. In the experiments, WC-CoCr was applied to an internal diameter of 150 mm and evaluated using a dedicated pin-on-disk wear test and standard axial fatigue tests. The results are presented and discussed along with the potential for further development of the inner diameter HVOF spraying technique.