Abstract
In this study, Cu-based bulk metallic glass coatings were deposited by atmospheric plasma spraying with different hydrogen flow rates. The crystallization and oxidation of the coatings is assessed along with corrosion resistance. As thermal energy in the plasma jet increases, the melting fraction and oxidation of particles in the coating increases as does porosity. All of these factors have an effect on the corrosion resistance of Cu-based bulk metallic glass coatings and their relative impact is discussed.