This paper provides a summary of the status and potential of thermal spray activities in Korea. It describes how various market sectors in Korea are using spray coating technology and presents annual sales estimates and share of market data broken out by industry, spraying technology, and patents awarded. It also reviews recent advancements in the development and use of thermal spray technology in Korea along with anticipated future impacts.