Abstract
This paper provides best practices along with a detailed example of how to effectively meet thermal spray training needs. It discusses the importance of giving students hands-on experience with real equipment and the many and varied problems they are likely to encounter with its use. It also discusses the value of allowing students to learn by exposing them to improper techniques, flawed approaches, and incorrect equipment repairs.