Nanocomposite epoxies are novel sealants developed especially for sealing metalized coatings. In order to test the corrosion protection performance of arc-sprayed aluminum coatings plus this sealer, steel panels were coated and placed in a corrosion test site on the East China Sea. Test panels were mounted in a marine atmosphere zone, seawater splash zone, tidal zone, and full-immersion zone. Several tests were conducted including corrosion and coating adhesion tests. This paper presents the results obtained from composite-coated steel panels after three years of seawater exposure.