Abstract
This paper presents some results of investigation of the cold spraying various composites including metal-ceramics, metal-metal with a new nozzle design. The objective of this study was to develop a nozzle with an ejector that allows the injection of powder components in different points of the gas flow that can provide optimal spray parameters for each component. For this purpose the installation was equipped with three feeders and three powder feed ports. The first one was located in a pre-chamber (high pressure powder feeder) and two others were located in the ejector in supersonic part of the nozzle. Varying the powder injection location of any component allowed us to change the spray parameters of the mixture. Some preliminary spray results of different powder mixtures are presented to illustrate possibilities of such approach. It is shown that an addition of ceramic or metal powder to the sprayed metal can significantly change the spray process and coating characteristics