We present the results of an investigation of the effects of a travelling magnetic field (TMF) on the plasma flow using a commercial program package. The argon plasma generation in the electric arc and the Lorentz force induced by the TMF are simulated with specific equations, which are derived from the magnetofluiddynamic equations using appropriate simplifications. First calculations confirm the predicted effects.