Abstract
High requirements of Cold Gas Dynamic Spray (GDS) process caused the development of low pressure DYMET technology. The technology and equipment evolution is presented and discussed. Modern portable low pressure DYMET equipment may be easily applied for various technical problem solutions. Multiple applications are briefly described.
Copyright © 2007 ASM International. All rights reserved.
2007
ASM International