Abstract
Thermal spraying for joining and filling of aluminum substrates under atmospheric conditions represents an enrichment in soldering technology. In a respective process, rod-, wire- or cored wire type, zinc-aluminum-based spray materials are applied for joining components or area filling of substrate and fused simultaneously. The advantages, in contrast to soldering, result from the direct application of the spray material, in particular also in constraint positions, and an uncomplex processing, which enables a conditioned inline capability and the use as a comparatively simple procedure for construction-site services or repairs. The aluminum substrate surface and spray material passivation, which would prevent a successful fusing, can be effectively suppressed by the use of a flux in the cored wires as well as straight on the substrates or a brushing activation.