Dynamic Metallization (DYMET) process is developed to produce thick aluminum, copper, zinc, nickel, cobalt, lead, and tin coatings on any metal or ceramic substrates. It consists of a surface treatment process in which a mixture of solid metal and ceramic powders are accelerated by compressed air at pressures between 0.5 and 0.8 MPa.