Real-time control offers the potential to reduce plasma spray variations that affect yield and coating quality. Important factors for designing such controllers are discussed including dominant nonlinearities, cross-coupling interactions, and sensor issues. The performance of several alternative strategies to achieve better coating thickness control are evaluated.