Abstract
The principles of system approach to modeling of sprayed particles interaction with substrate in process of thermal spraying of coatings are discussed. The proposed model have six levels for analysis of particle-substrate interaction system: functional, technological, mechanical interaction, thermal, mass transfer level, and metallophysics level.
This content is only available as a PDF.