Abstract
Research and selection the performance requirements for the coating, at the same time obtain the WC-Co powders with high efficient spray rate and low cost, through research on the relation between the WC-Co powders sprayed by the HVOF in different morphology and in different manufacturing process and the spraying parameters and structures of coatings. Abstract only; no full-text paper available.