With the incoming of HVOF, the coating properties and application extent of WC-Co type have been greatly improved, in the recent years, we found that the characteristics of WC-Co powder has some influence on its coating properties prepared by HVOF. In this paper, study has been prepared on powders made from aboard and Beijing General Research Institute of Mining & Metallurgy properties such as fluidity, aspect, profile of coating SEM and carbon content, also phase structure and properties analysis of HVOF coating has been made. Finally, influence of powder preparing technology and HVOF technology parameters of different powders for coating properties have been described.