Abstract
Extensive research activities were conducted over the last few years on coatings made of titanium oxide, an established material for thermally sprayed coating solutions. Multiple existing and potential applications are closely connected with the existence of different titanium dioxide modifications and the formation of suboxides. This provides a basis for discussions on the Ti-O phase diagram as well as the properties and conditions of formation of relevant phases. Coating microstructures, phase compositions and mechanical properties are discussed as a result of interactions of different spray powders in different spray conditions of atmospheric and vacuum plasma spraying (APS and VPS), as well as of high-velocity oxyfuel (HVOF) spraying. The discussion on applications is focused on electrically conductive coatings, coatings with photocatalytic properties and coatings for wear applications.