Northwest Mettech Corporation has recently developed a new high power torch for spraying internal surfaces, the Axial III ID. The Axial III ID has been successfully operating at 135 kW while spraying inside a drum with an inner diameter of 34 cm. The three-electrode axial injection configuration of the new torch is based on the current Axial III torch. Various coatings were sprayed inside a drum while monitoring the torch temperature. The results of these experiments are presented in this paper.