Thermal spray coatings exhibit a wide variety of microstructural characteristics that lead to variation in their functional properties. A complete understanding of the plasma spray process includes examination of the particle-flame interaction, particle impact (to form the splats), and the particle-substrate interaction during coating deposition. The links between these process parameters and coating properties has been established by using diagnostic tools in conjunction with a splat collection shutter and an in-situ curvature measurement instrument. In this study, a commercial grade molybdenum (Mo) powder was plasma sprayed; the spray stream was characterized in relation to the resulting particle state. A "splat map" was deposited through a "spray stream guillotine" to capture the fingerprint of the plume cross section. Subsequently, coatings were deposited at these spray conditions on a newly developed in-situ curvature measurement instrument to measure coating stresses and to estimate the coating modulus. Splats and coatings were subsequently characterized by micro-diffraction (for splat residual stresses), by nano and micro-indentation for elastic and elastic-plastic properties, and by electron microscopy. This complete history of the process followed by splat and coating characterization provides insight into the correlation between processing parameters, resultant particle states, and final coating properties. The role of particle temperature and velocity on the splat (and coating) morphology and residual stress is explained in the results.

This content is only available as a PDF.
You do not currently have access to this content.