The effect of methods and conditions of thermal spraying on structure and phase composition of coatings of the Al-Cu-Fe system alloy powders has been investigated. It is shown that the maximum ø-phase content of the coatings can be produced by the method of air-gas plasma spraying. In this case the thermal spray coatings inherit the multi-phase nature of initial powders. Preheating of the substrate prior to spraying allows the ø-phase content of the coatings to be increased.