A laminated coating, using the thermal spray and other processes, protects a metal substrate in a highly corrosive and highly erosive environment. The combination of noble metals and ceramics offer highly bonded, pore free coatings for demanding industrial applications. This paper offers case examples to exemplify some success stories.