Industrial gas product supply has a dramatic influence on the quality, consistency, and performance of thermal spray coatings and their application equipment. The various thermal spray processes test the limits of common gas supply modes in the areas of safety, pressure, purity, storage, and recovery. Selection criteria for the gas and supply mode, using the latest methods, are discussed for plasma, HVOF and cold spray techniques.