Abstract
This paper describes a new spraying process that uses a special torch to inject aluminum oxide suspensions into a dc plasma jet. Based on the results obtained, a general mechanism of action is proposed in which factors such as acceleration, impact behavior, and heat transfer phenomena play a role. Paper includes a German-language abstract.