In this paper, Hastelloy C-276 layers are produced using the Axial III plasma spray method and assessed based on oxide content and microhardness. Test results show that Hastelloy coatings with low hardness can be achieved in different atmospheres with appropriate adjustments in process parameters. Paper includes a German-language abstract.