Abstract
This paper introduces a new three-cathode plasma burner and explains how it functions in comparison to conventional plasma guns. Paper text in German.
This content is only available as a PDF.
Copyright © 2002 Verlag für Schweißen und verwandte Verfahren DVS-Verlag GmbH. All rights reserved.
2002
Verlag für Schweißen und verwandte Verfahren DVS-Verlag GmbH
Issue Section:
Atmospheric Plasma Spraying Processes