Thermal Spray 2025: Proceedings from the International Thermal Spray Conference
Cold Sprayed or Aerosol Deposition: Metals, Polymers, Ceramics, and Metal Matrix Composite Coatings
Thermal and Environmental Barrier Coatings for Gas Turbines
Effects of Various Air Plasma Spraying Processes on the Spraying Power and Bond Strength of Yb2Si2O7/Si-HfO2 Environmental Barrier Coatings
Kaibin Li; Weize Wang; Shilong Yang; Yangguang Liu; Hongchen Li; Wenkang Zhang; Changliang Wang; Xiuxin Du
ITSC 2025; 15-22https://doi.org/10.31399/asm.cp.itsc2025p0015
Wear and Corrosion Protection Applications
Pre-Oxidized High-Velocity Oxygen Fuel Sprayed CoNiCrAlY Coating as An Environmental Barrier Against Ammonia Corrosion for Pure Ammonia Combustion Gas Turbines
Tina Ghara; Seiji Kuroda; Takashi Yanagisawa; Mohammed Shahien; Kentaro Shinoda; Masato Suzuki; Takahiro Inoue
ITSC 2025; 450-456https://doi.org/10.31399/asm.cp.itsc2025p0450
Cold Spray Process Fundamentals, Simulation, and Particle Impact
Novel Coatings
Plasma Sprayed Wear-Resistant, Low-Friction, and Non-Stick Quasicrystalline Al-Cu-Fe Coatings
Ingor Baumann; Jonas Zajaczkowski; Mukul Aravind Kada; Dennis Kensy; Wolfgang Tillmann; Monika Kipp; Jannis Saelzer; Dirk Biermann; Marko Sipura; Nenad Piljic
ITSC 2025; 105-111https://doi.org/10.31399/asm.cp.itsc2025p0105
Equipment, Powder, Consumables, and Economics
Optimizing a Modular Cascaded Plasma Torch to Manufacture Dense Alumina Coatings with High Spray Efficiency
Myriam Sleiman; Geoffrey Darut; Ralph Seulin; Marie Pierre Planche; Jean-Jacques Gonzalez; Pierre Freton; Francis Sambou; Armando Salito; Manfred Rösli
ITSC 2025; 129-136https://doi.org/10.31399/asm.cp.itsc2025p0129