ISTFA2021, ISTFA 2021: Conference Proceedings from the 47th International Symposium for Testing and Failure Analysis, 263-268, October 31–November 4, 2021,
.... Because the standard deviation in the two algorithms is over-estimated in wafer level test distribution, the two algorithms fail to represent the size of difference for the two samples exactly. Therefore, we introduce quantile comparison equivalence criteria (QCEC) which is robust to overall data...