Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Embrittlement
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
Characterization of Gold Embrittlement in Solder Joints
Available to Purchase
ISTFA1999, ISTFA 1999: Conference Proceedings from the 25th International Symposium for Testing and Failure Analysis, 305-308, November 14–18, 1999,
Abstract
View Papertitled, Characterization of Gold Embrittlement in Solder Joints
View
PDF
for content titled, Characterization of Gold Embrittlement in Solder Joints
Mechanical strength, integrity, and reliability of solder connections used in the microelectronics industry are important factors in overall quality and reliability of the finished product. In most cases tin (Sn) rich solders are attached to a base metal plated with nickel (Ni) and then with gold (Au). Formation of AuSn4 intermetallics in the solder may result in loss of more than 80% of the initial impact toughness, resulting in loss of reliability of the connection. Gold (Au) embrittlement is a major concern in tin/lead (Sn/Pb) soldering or any other joining process with Au and Sn as major constituents. Noncompliance to Au plating-thickness specifications by vendors or insufficient Sn wicking of Au surfaces can result in embrittled joints and unreliable parts.