Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Article Type
Volume Subject Area
Date
Availability
1-1 of 1
Matthew Mulholland
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Proceedings Papers
ISTFA2015, ISTFA 2015: Conference Proceedings from the 41st International Symposium for Testing and Failure Analysis, 466-473, November 1–5, 2015,
Abstract
PDF
Abstract The X-ray inspection of fully assembled samples is becoming ever more important as the benefits of using area array packages/chip scale packages/flip chips are applied to more and more products. Sample preparation has traditionally been used to improve access to geometry or a specific location with a known defect that requires verification. The novel paradigm is an integrated approach to sample preparation and X-ray inspection to optimize resolution and throughput time performance with minimally deprocessed sample. This paper, covering the limitations of X-Ray imaging and 3D tomographic reconstruction, discusses the development of models for throughput time and resolution by failure analysis labs. It also discusses the processes involved in advanced sample preparation techniques and global BGA removal to obtain improved resolution at die level.