This research summarizes a variety of physical failure modes of GaAs-based oxide-confined VCSELs and their root causes. Standard failure analysis procedure, which includes defect fault isolation by PEM or IR-OBIRCH and physical inspection by TEM analysis are also presented in detail.

This content is only available as a PDF.