This paper demonstrates a novel defect localization approach based on EBIRCH isolation conducted from the backside of flip chips. It discusses sample preparation and probing considerations and presents a case study that shows how the technique makes it possible to determine the root cause of subtle defects, such as bridging, in flip chip failures.