In advanced chip package failure investigations, Electro Optical Terahertz Pulse Reflectometry (EOTPR) simulation emerges as a highly effective fault isolation technique. However, traditional manual methods for generating simulation models face significant challenges, including laboriousness, time consumption, and susceptibility to human error. To address these obstacles, we have developed an automation software script in-house. This script autonomously interfaces with the design database, extracting crucial trace information and generating an optimized equivalent trace model. This automated process markedly enhances the efficiency of EOTPR model simulations, streamlining workflow, standardizing procedures, and reducing the potential for human error. The efficacy of integrating the automation script into the workflow of advanced package failure analysis was demonstrated through two case studies. This integration significantly enhanced productivity and enabled successful root-cause investigation of advanced package failures.

This content is only available as a PDF.
You do not currently have access to this content.